> they immediately painted the shell with Ditzler DP40 primer. This is a rust > inhibiting primer that seals out moisture. > If you read the instructions for DP40 you will find that a top coat should be applied within 7 days. Supposedly DP40 can be scuff sanded after this time for good adhesion but this could be a problem in hard to get to areas. Roland |